Nanoseminar
Group of Structure analysis at the Department of Condensed Matter Physics
of Charles University and MGML has a pleasure to invite you to attend the seminar on nanomaterials: Physics, Technology, Applications
on 5th November 2026 at 14:00
at Faculty of Mathematics and Physics of Charles University, Ke Karlovu 5, 121 16 Praha 2
Lecture room F2
Somnath Dey, Lukáš Palatinus
Institute of Physics of the Czech Academy of Sciences
Application of 3D electron diffraction to probe deformations in mechanically flexible molecular crystals
Somnath Dey, Lukáš Palatinus » Application of 3D electron diffraction to probe deformations in mechanically flexible molecular crystals
Institute of Physics of the Czech Academy of Sciences
*corresponding author: e-mail: dey@fzu.cz, palat@fzu.cz
Location: Lecture room F2 (MFF UK, Ke Karlovu 5)
Molecular crystals with macroscopic flexibility have shown tremendous potential for applications as flexible optical waveguides, fluorescent materials, piezo- and ferroelectrics, semiconductors and drug tablets.[1 and references therein] μ X-ray diffraction employing synchrotron has been used to understand the underlying mechanisms of deformation.[2] However, inherent disadvantages of the method preclude quantification of underlying defects under strain.
Electrons interact with matter 104 times more than X-ray. By means of a transmission electron microscope (TEM), diffraction experiments can be performed on sub-micron sized crystals to elucidate their crystal structures.[3] Therefore, electron diffraction can be used to determine spatially resolved crystal structures from deformed crystals. In addition, the dynamical refinement approach readily resolves crystal thickness and absolute structures.[4,5]
Two classes of materials are chosen, viz. plastically flexible crystals of hexachlorobenzene[6] and elastically flexible cocrystal solvates of caffeine.[7] Deformations in these materials were investigated by continuous rotation 3D electron diffraction (3DED) experiments using the TEM FEI Tecnai G2 20 equipped with a hybrid pixel detector at T = 100 K. Several points were mapped on micro-rod shaped crystals. At each point 3DED images were collected using conditions: -45° ≤ α ≤ 35°, Δα = 0.3°, exposure t ≤ 400 ms.
We present the mechanism of deformations in these materials that involves variations in intermolecular distances and rotations as a function of different regions. Crucially, the investigations help us realise the mechanical limits of these materials.
References:
[1] Z. Zhou et al. (2022) Chem. Eng J. 450, 138333.
[2] A. J. Thompson et al. (2021) CrystEngComm 23, 5731.
[3] M. Gemmi et al. (2019) ACS Cent. Sci. 5, 1315–1329.
[4] L. Palatinus et al. (2015) (a) Acta Crystallogr. A 71, 235-244; (b) Acta Crystallogr. B 71, 740-751.
[5] P. B. Klar et al. (2023) Nat. Chem. 15, 848–855
[6] M. K. Panda et al. (2015) Nat. Chem. 7, 65-72.
[7] S. Ghosh et al. (2012) Angew. Chem. Int. Ed. 51, 10319
The authors acknowledge P4F MSCA COFUND reg. nr: 101081515 for funding.